Another benefit from OKULEN®: we perform all of our tests at our own production-independent lab.
- Charpy double-notch impact strength according to DIN EN ISO 21304-2
- Wear according to DIN EN ISO 15527 (sand slurry method)
- Hardness according to DIN EN ISO 868
- Yield stress according to DIN EN ISO 527-2 (ASTM D638)
- Stretch-elastic modulus according to DIN EN ISO 527-2 (ASTM D638)
- Breaking/tensile strength according to DIN-EN-ISO 527-2 (ASTM D638)
- Stretch at break according to DIN EN ISO 527-2 (ASTM D638)
- Surface resistivity and volume resistivity according to DIN-EN 62631-3-2 and DIN-EN 62631-3-1
- Mass melt flow rate (MFR) according to DIN EN ISO 1133-1
- Differential scanning calorimetry (DSC) according to DIN EN ISO 11357-1
- Density according to DIN-EN-ISO 1183-1
- Static and dynamic friction coefficient according to DIN EN ISO 8295 (ASTM D1894)
- Ball indentation hardness to DIN-EN-ISO 2039-1